電磁純鐵退火工藝與溫度
The DT4E pure iron was annealed at the temperatures of 800-1 000 ℃ for the holding time of 180-360 min. Then the effects of annealing process on the grain sizes, magnetic properties and tensile strength of the pure iron were studied and the optimum annealing process was determined. The results show that the grain size of the annealed pure iron increased with the increase of holding time, and first increased then decreased then increased with the increase of the temperature. With the increase of grain size, the magnetic induction of the pure iron increased while the coercivity and tensile strength decreased. The recommended annealing process was at 850 ℃ for 240-300 min.







溫馨提示:以上是關于重慶1215+C退火棒現貨 蘇州安達龍的詳細介紹,產品由蘇州安達龍金屬材料有限公司為您提供,如果您對蘇州安達龍金屬材料有限公司產品信息感興趣可以聯系供應商或者讓供應商主動聯系您 ,您也可以查看更多與特殊鋼相關的產品!
免責聲明:以上信息由會員自行提供,內容的真實性、準確性和合法性由發布會員負責,天助網對此不承擔任何責任。天助網不涉及用戶間因交易而產生的法律關系及法律糾紛, 糾紛由您自行協商解決。
風險提醒:本網站僅作為用戶尋找交易對象,就貨物和服務的交易進行協商,以及獲取各類與貿易相關的服務信息的平臺。為避免產生購買風險,建議您在購買相關產品前務必 確認供應商資質及產品質量。過低的價格、夸張的描述、私人銀行賬戶等都有可能是虛假信息,請采購商謹慎對待,謹防欺詐,對于任何付款行為請您慎重抉擇!如您遇到欺詐 等不誠信行為,請您立即與天助網聯系,如查證屬實,天助網會對該企業商鋪做注銷處理,但天助網不對您因此造成的損失承擔責任!
聯系:tousu@tz1288.com是處理侵權投訴的專用郵箱,在您的合法權益受到侵害時,歡迎您向該郵箱發送郵件,我們會在3個工作日內給您答復,感謝您對我們的關注與支持!